Silica-alumina solid waste-based composite cementitious materials are produced using industrial solid wastes such as fly ash, slag, steel slag, coal gangue, and red mud. The process involves combining different waste materials and activating their reactive components so that the available silica and alumina participate in cementitious reactions. The resulting material develops strength and structural stability.
Different solid wastes vary in chemical composition, mineral structure, and reactivity. Their proportions should therefore not be determined by a fixed formula. Before production, the raw materials need to be tested and evaluated for their reactivity. The mix proportions, activator type, grinding fineness, and curing conditions can then be selected according to the intended application.
The main production stages include raw material selection and pre-treatment, mix proportion design, grinding and activation, blending and homogenization, followed by reaction curing and product testing.
Raw Material Selection and Pre-treatment
Raw material quality directly affects the reactivity, setting time, and final strength of the cementitious material. Before production, solid wastes should be selected according to their composition and intended use, followed by the necessary pre-treatment.
Raw Material Selection and Composition Analysis
Common raw materials include:
Fly ash: Contains reactive silica and alumina and is commonly used in alkali-activated and composite cementitious systems.
Granulated blast-furnace slag: Contains reactive calcium, silica, and alumina. It has latent hydraulic properties and is often blended with fly ash and other materials.
Steel slag: Contains calcium, silicon, iron, and other components. It can be used as a raw material in composite cementitious systems, but free calcium oxide, magnesium oxide, and volume stability must be considered.
Coal gangue: Contains silica-alumina minerals. Some types require calcination to improve their reactivity before use.
Red mud: Contains iron, aluminum, silicon, calcium, and alkaline components. It can be blended with other solid wastes according to its chemical composition.
Raw material selection should not rely solely on the total SiO₂ and Al₂O₃ content. Other parameters, including CaO, MgO, Fe₂O₃, SO₃, and loss on ignition, should also be tested. X-ray diffraction (XRD) can be used to examine the mineral composition and amorphous phase content.
For industrial solid wastes containing heavy metals or soluble salts, appropriate leaching tests and environmental safety assessments are also necessary.
The content of reactive silica and alumina, together with the mineral structure of the raw materials, affects their response to activation. A single minimum threshold for total reactive silica and alumina should therefore not be applied to all types of solid waste.
Crushing, Screening, and Drying
Bulky or coarse solid waste should first undergo crushing. Jaw crushers and impact crushers are commonly used for this purpose. The crushed materials can then pass through vibrating screens to remove oversized particles and other impurities.
The pre-treated materials may also require drying, depending on their moisture content. Rotary kilns and fluidized-bed dryers are suitable options for materials with high moisture content that may interfere with grinding and homogenization.
The target moisture content should be determined according to the raw material properties, grinding process, and storage requirements. A moisture content of 1% or less should not be treated as a universal requirement for every type of solid waste.
Special Activation of Certain Solid Wastes
Some solid wastes do not develop sufficient reactivity through ordinary crushing and grinding alone. In these cases, additional treatment may be necessary.
For example, some of the silica-alumina minerals in coal gangue have crystalline structures. Calcination can change these structures and improve their reactivity in subsequent cementitious reactions.
According to T/GRM 117-2025, the specific surface area of coal gangue powder used in coal-based geopolymer production should be approximately 350 m²/kg ± 20 m²/kg. The standard also specifies calcination at temperatures above 650°C for at least 2 h to activate the material. These requirements apply to the coal-based solid waste systems covered by the standard and should not be directly applied to other raw materials.
For red mud, particular attention should be paid to its alkali content and soluble salts. Whether washing, dealkalization, or another pre-treatment method is necessary depends on its composition, the mix design, and the required properties of the final product. The alkaline components in red mud may also contribute to activation in certain alkali-activated systems, so pre-treatment to remove alkali is not always required.
Raw Material Blending and Mix Proportion Design
Mix proportion design has a major influence on the properties of composite cementitious materials. The proportions of different solid wastes should be selected according to their chemical compositions and complementary characteristics, as well as the required strength, setting time, workability, and durability.
Determining the Proportions of Solid Waste Components
Common blending approaches include:
Slag and fly ash: Combines the latent hydraulic properties of slag with the silica-alumina components of fly ash to form a composite cementitious system.
Coal gangue and fly ash: Uses calcination and alkali activation where necessary to improve the resource utilization of coal-based solid wastes.
Steel slag and slag: Combines their calcium and silicon components to adjust the reaction characteristics of the cementitious system.
Red mud and fly ash or slag: Uses differences in alkali content and silica-alumina composition to determine the activator dosage and overall mix proportions.
Selecting Activators and Determining Their Dosage
In alkali-activated cementitious materials, activators promote the dissolution of reactive silica and alumina in solid waste, allowing these components to participate in subsequent reactions.
Common activators include:
Waterglass-based activators: Usually based on sodium silicate or potassium silicate, often combined with sodium hydroxide or potassium hydroxide.
Alkaline activators: Include sodium hydroxide, potassium hydroxide, and lime. The choice depends on the raw material composition and reaction system.
Sulfate-based components: Include gypsum and anhydrous sodium sulfate. These can be used in certain slag-based or composite activation systems.
The activator type, concentration, and dosage should be determined according to the chemical composition and reactivity of the solid waste. For waterglass-based activators, the modulus, expressed as the molar ratio of SiO₂ to Na₂O, also needs to be controlled.
The 5% to 15% total activator dosage mentioned in the original material should not be treated as a standard proportion for all systems. The calculation must identify the activator composition, effective alkali content, and reference mass used to determine the dosage.
For example, T/GRM 117-2025 specifies different sodium silicate or potassium silicate dosage ranges for different coal-based geopolymer systems:
Coal gangue-based geopolymers: 9% to 15% of the coal gangue mass.
Fly ash-based geopolymers: 5% to 10% of the fly ash mass.
Multi-source coal-based solid waste geopolymers: 6% to 12% of the total coal-based solid waste mass.
These values apply to the specific coal-based solid waste systems covered by the standard. They are not general mix proportions for all silica-alumina solid waste-based cementitious materials.
Selecting Chemical Admixtures
Depending on the application and construction requirements, admixtures such as water reducers and retarders may be added to improve workability or adjust setting time.
The type and dosage of each admixture should be determined through compatibility testing. Different alkali-activated systems respond differently to chemical admixtures, so dosage recommendations for ordinary Portland cement should not be applied directly.
Grinding, Activation, and Fineness Control
Grinding reduces particle size and increases specific surface area. It also improves the uniformity of the raw material mixture and provides suitable particle conditions for subsequent cementitious reactions.
Selecting Grinding Equipment
Ball mills and vertical roller mills can be selected according to raw material hardness, initial particle size, and production capacity.
Different solid waste materials can be ground separately and then blended, or processed together through co-grinding, depending on their properties.
Separate grinding allows the fineness of each material to be controlled independently before blending according to the mix design. Co-grinding combines different raw materials during the grinding process, but differences in grindability must be considered to prevent uneven particle size distribution.
Controlling Grinding Fineness
Specific surface area affects the reactivity of solid waste particles and the performance of cementitious materials. However, the optimum fineness varies among different raw materials.
The specific surface areas of at least 400 m²/kg for slag and 350 m²/kg for fly ash, as mentioned in the original material, can be used as initial reference values during mix development. They should not be treated as universal requirements for all solid waste-based cementitious materials.
The required fineness should be determined through grinding trials and mortar strength tests. For materials with relatively low reactivity, such as coal gangue, the effect of calcination activation should also be considered. Increasing grinding time alone may not be an effective way to improve material reactivity.
Controlling Grinding Temperature
The temperature inside the grinding equipment and at the material outlet should be monitored. Excessive heat may cause dehydration or changes in the phase composition of certain sulfate-containing components, which can affect the setting and hardening properties of the cementitious material.
For composite systems containing gypsum, temperature control should account for the type of gypsum, grinding time, and mix design. The limit of 80°C or lower mentioned in the original material can serve as a reference for certain processes, but it should not be treated as a universal temperature limit for all formulations and equipment.
Homogenization, Mixing, Forming, and Curing
After grinding, the mixing process should be selected according to the product form and activation method. Dry powder binders and alkali-activated materials prepared at the construction site do not necessarily follow the same production sequence.
Dry Blending and Homogenization
For pre-blended dry powder products, the ground solid waste materials, solid activators, and suitable powdered admixtures can be fed into a mixer according to the mix proportions.
Mixing time depends on the equipment type, loading volume, and material dispersion. The 5 to 10 minute period mentioned in the original material can be used as an initial reference during process trials. Actual production settings should be determined through mixing uniformity tests.
For systems that use liquid activators, the liquid activator should not simply be added to the grinding equipment for co-grinding with the solid materials. The activator solution is generally prepared and stored separately, then mixed with the solid raw materials during use.
Water Addition and Activation
For one-component dry powder products, water is generally added according to the mix design during construction or use.
For two-component systems that use liquid activators, the activator solution and any additional mixing water must be added according to the specified proportions. The materials are then mixed until the components are evenly dispersed and the reaction can proceed.
Water content and activator concentration need to be controlled during mixing. Excessive water can increase porosity and reduce the strength and durability of the hardened material. Insufficient water may prevent proper dispersion and affect workability.
Forming and Curing
After mixing, the material is cast or pressed into the required shape. Natural curing or controlled heat curing can then be selected according to the cementitious system.
Temperature and humidity should be controlled during curing to support continued cementitious reactions. Setting and hardening rates vary with the solid waste composition and activator system, so the curing conditions should be established through testing.
For example, T/GRM 117-2025 recommends at least 7 days of temperature-controlled and moisture-retaining curing for coal-based solid waste geopolymers under natural curing conditions. This requirement applies to the geopolymer systems covered by the standard. Other material systems require curing schedules based on their own performance requirements.
Product Testing and Production Considerations
After preparation, product quality should not be assessed solely by appearance or grinding fineness. Both fresh and hardened material properties need to be tested.
Main Quality Control Tests
Setting time: Initial and final setting times are measured to determine whether the material meets construction and forming requirements.
Strength: Compressive and flexural strength tests using mortar or specified test specimens are used to evaluate strength development.
Soundness: Testing checks whether the material undergoes undesirable volume changes during hardening.
Durability: Depending on the intended service environment, testing may include permeability, chemical resistance, and long-term performance.
Environmental safety: For solid waste containing heavy metals or other potentially harmful substances, leaching tests should be conducted to assess the environmental safety of the finished product.
Production Considerations
Solid wastes from different sources can vary considerably in chemical composition and reactivity. Raw material testing, trial batching, and mortar strength testing are necessary before finalizing the mix proportions.
For highly alkaline materials such as red mud, soluble alkali and salt content should be evaluated. Whether pre-treatment is necessary depends on the risk of efflorescence and the required setting and durability properties.
For steel slag, free CaO and MgO must be considered because they can cause volume instability. Calcium content alone is not sufficient to assess its suitability.
When using alkaline activators such as sodium hydroxide and potassium hydroxide, suitable corrosion-resistant storage, metering, and conveying systems must be provided. Operators also need appropriate protective equipment.
Water content during construction should be controlled according to the specific cementitious system. The water-to-binder ratio of 0.4 to 0.55 mentioned in the original material should not be treated as a universal requirement. For coal-based solid waste geopolymers, T/GRM 117-2025 gives a reference mass ratio of water to coal-based solid waste feedstock of 0.25 to 0.55. The actual value should be determined according to the mix design.
Custom Machining for Solid Waste-Based Cementitious Material Production Equipment
The production of silica-alumina solid waste-based composite cementitious materials involves several processes, including crushing, screening, drying, grinding, mixing, and conveying. Transmission components, support parts, and non-standard structural components used in different machines must meet the relevant dimensional and assembly requirements.
We provide custom precision machining for these production machines based on customer-supplied drawings. Single-piece and small-batch manufacturing are available. Machining processes and production requirements are determined according to the component drawings and assembly specifications.
Conclusion
The preparation of silica-alumina solid waste-based composite cementitious materials requires the raw material proportions, activator system, and grinding fineness to be selected according to the chemical composition and reactivity of each solid waste. After suitable pre-treatment, blending, grinding, and homogenization, the materials undergo water addition and activation, forming, curing, and performance testing to ensure that they meet the required strength, soundness, and durability standards.
Beyond components for solid waste processing and building material production equipment, Hansheng Automation also provides custom precision machining for other industries. Our machining services cover precision parts for yacht equipment, structural components for radio-controlled racing cars, and non-standard parts for tobacco packaging machinery and filling machinery. We support single-piece and small-batch production according to customer drawings and specific machining requirements.